Basit öğe kaydını göster

dc.contributor.authorDoğan, Mehmet Akif
dc.contributor.authorGemi, Lokman
dc.contributor.authorYazman, Şakir
dc.contributor.authorCeritbinmez, Ferhat
dc.contributor.authorYapıcı, Ahmet
dc.date.accessioned2025-01-27T11:17:06Z
dc.date.available2025-01-27T11:17:06Z
dc.date.issued2024en_US
dc.identifier.citationDoğan, M.A., Gemi, L., Yazman, Ceritbinmez, F., Yapici, A. (2024). Effect of hybridization and stacking sequence on damage development in AWJ machining of Al/FRP/Al FML composites. Journal of Manufacturing Processes, 131, pp. 141-159. https://doi.org/10.1016/j.jmapro.2024.09.017en_US
dc.identifier.issn1526-6125
dc.identifier.issn2212-4616
dc.identifier.urihttps://doi.org/10.1016/j.jmapro.2024.09.017
dc.identifier.urihttps://hdl.handle.net/20.500.12508/3210
dc.description.abstractIn this study, 5 different Al2024/FRP/Al2024 metal stacked composites were produced and their machinability by abrasive water jet machining (AWJM) method was investigated. Synergistic interaction of these materials offers new and improved properties, but machinability remains an area of research due to widely varying mechanical properties. The effects of different stacking and traverse speed on hole quality in cutting with AWJM were determined. The hole diameter deviation (HDD) ratio, kerf, delamination, hole circularity, and surface morphology were analyzed. Result of the current study showed that the increase in traverse speed caused an increase in the HDD ratio, in the visibility of the cutting starting point, in the deviation of circularity, and in the bore-hole damage formation. In all stacks with CFRP, an average deviation of 5 % at the hole entrance and 4 % at the hole exit occurred at a traverse speed of 1000 mm/min. At 400 and 600 mm/min traverse speeds, an average of 2.8 % deviation occurred at the hole entrance and an average of 2.13 % at the hole exit. This proves that the traverse speed has a significant effect on the hole diameter. In addition, as the traverse speed decreased, it was noticed that the layers separated from each other, causing delamination, and therefore the thickness of the FML increased. Different defects were observed to occur in FRP structures used in FML with SEM analysis. Intralayer defects were more dominant in GFRP laminate, whereas interlayer defects were found to form in CFRP laminate.en_US
dc.language.isoengen_US
dc.publisherElsevieren_US
dc.relation.isversionof10.1016/j.jmapro.2024.09.017en_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectMachinabilityen_US
dc.subjectMetal cuttingen_US
dc.subject.classificationReinforced Plastic
dc.subject.classificationDelamination
dc.subject.classificationMachining
dc.subject.classificationEngineering, Manufacturing
dc.subject.classificationEngineering & Materials Science - Manufacturing - Tool Wear
dc.subject.otherMachinability
dc.subject.otherMetal cutting
dc.subject.otherAbrasive water jet machining
dc.subject.otherDamage development
dc.subject.otherDamage-mechanics
dc.subject.otherHole diameter
dc.subject.otherHybrid
dc.subject.otherHybridisation
dc.subject.otherMachining methods
dc.subject.otherProperty
dc.subject.otherStacking sequence
dc.subject.otherTraverse speed
dc.subject.otherDelamination
dc.titleEffect of hybridization and stacking sequence on damage development in AWJ machining of Al/FRP/Al FML compositesen_US
dc.typearticleen_US
dc.relation.journalJournal of Manufacturing Processesen_US
dc.contributor.departmentErzin Organize Sanayi Bölgesi (OSB) Meslek Yüksekokulu -- Makine Bölümüen_US
dc.contributor.departmentMühendislik ve Doğa Bilimleri Fakültesi -- Makina Mühendisliği Bölümü
dc.identifier.volume131en_US
dc.identifier.startpage141en_US
dc.identifier.endpage159en_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.contributor.isteauthorDoğan, Mehmet Akif
dc.contributor.isteauthorYapıcı, Ahmet
dc.relation.indexWeb of Science - Scopusen_US
dc.relation.indexWeb of Science Core Collection - Science Citation Index Expanded


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster